With lead secured, you need a way to heat it up and clean it. This is the smelting process. You can go straight into the casting mode from wheel weights, but I don't advise it as the additional cleaning and manipulation that needs to be done to the melt really prevents you from hitting a good bullet producing rhythm.
As you heat the lead up, you will need several more things, first- a way of removing debris from the lead. For this I like a slotted spoon. Second- you will need a way of transferring the lead from the smelting pot to a mold, as the pot itself is unwieldy, and that would be a huge waste of heat resources. I use a cast iron ladle. Both the slotted spoon and ladle cost me a total of $1 dollar at a yard sale.
After you have the molten lead free of foreign matter, you need to 'flux' the lead to pull out impurities. You can buy flux, and it works well. I use saw-dust. It was free and as long as it is dry, it works great. The dry part is very important. Lead will react very poorly to water in its molten state, and you need to NEVER get molten lead and water into the same work space. The reaction is an energetic 'explosion' where the water quickly converts from a liquid to a gaseous state, expanding quickly in volume. If that water is under the surface of the melt, it will displace the liquid 800 degree lead so that it may expand more freely.
With fluxing out of the way, your melt will be a clean, shiny silver. We now need a container in which to place the molten lead to let it cool. You can be cheap here and use something like old tuna cans, but honestly I don't think it is advisable. I spent 50 cents and got an old muffin tin at a yard sale. My other ingot molds were made by a caster on the CASTBOOLITS forum. I honestly forgot what I spent on them, but you really don't need as many as I have. The muffin tin worked fine as my only ingot mold for a couple years and is still going strong.
You will notice when ladling lead, you never remove all the lead from your smelting pot. This is a good thing. That liquid lead allows you the maximum amount of surface area possible when adding more, not yet molten lead to your pot. I usually drain my pot 2/3 of the way before refilling with more wheel weights.
For just over two hours worth of work, I was rewarded with about 100 lbs of clean, usable lead ingots. depending on the weight of the bullet I cast, this will yield approximately 3.2-6.5k bullets. Casting the actual bullet takes me just over 2 hours per 1,000 bullets (using 6 cavity molds, and no I do not cast quickly) start to finish. Sizing the bullets takes another hour per 1,000.
Just as an investment of time, you can expect 4 hours to go from bucket to ready to load bullets per 1,000 projectiles you intend to create. That is based on the time it takes me to smelt, cast, and size projectiles.
25 bucks for the lead
40 bucks for the turkey fryer
00.50 for the ingot mold
01 for the skimming equipment
03 in propane / fuel
All told, 69.50 for 100 lbs of clean, usable lead ready to go for bullets. That amortizes out the full cost of equipment in the first shot, and then subsequent smelts need only cost you the fuel plus the price of the lead.
That means that my cost (with my equipment having long since paid for itself) is actually only 28 dollars for 100 lbs of clean usable lead. So for about the cost of 1,000 factory lead bullets, you can reasonably expect to set yourself up with significantly more lead than is needed to produce that many projectiles, and also absorb all the associated costs with the set up. This does not cost the price of bullet molds though- which we will cover in the next installment of this series.